Technical index Category |
Amino baking varnish (Generally) |
Acrylic baking varnish (High-grade) |
Main components |
Alkyd resin,Aminoresin, Additive |
Thermosetting acrylicresin,Amion resin Additive |
Drying conditions |
Semi-dry |
80~100℃/10~15min |
80~100℃/10~15min |
Completed-dry |
120~130℃/20~25min |
120~130℃/20~25min |
Sparying methods |
Wet-on-wet |
8-10min/air dry,sparying |
8-10min/air dry,sparying |
Wet-on-semidry |
Direct construction |
Direct construction |
Wet-on-completed dyr |
Construct cautiously,payattention to adhesion of interlayer |
Construct cautiously,payattention to adhesion of interlay |
Adhesion of every substrate |
Iron castings |
After pre-treatment,adhesion well |
After pre-treatment,adhesion well |
Aluminum parts |
Customizd if customer requires |
Customizd if customer requires |
Electroplated parts |
No adhesion,cant construct |
No adhesion,cant construct |
Lustre(60°lustremeter) |
≥95° |
≥95° |
Pencil hardness |
HB-H |
H-3H |
Impact enfurance test resistance kg/cm |
≥40 |
≥50 |
Solvent resistance |
Good |
Excellent |
Diluent |
Manual:xylene Electrostatic:electrostatic special thinner |
Using appointed matching diluent |
Remark |
If customers have specific reqirements,please contact the teminal selling or engineers of modern company to customize |